Problems With The Inner Wall Of F1960 Fittings

  • The inner wall of F1960 Fittings is rough: it may be the core rod temperature is too low; the body temperature is too low; the screw temperature is too high.

    There are cracks on the inner wall of F1960 Fittings: the material may have impurities; the core rod temperature is too low; the body temperature is low; the traction speed is too fast.

    The inner wall of F1960 Fittings is uneven: the temperature of the screw may be too high; the screw speed is too fast.

    There are bubbles on the inner wall of PEX Fittings Wholesale: it may be damp.